Main product:
Ø IN718 , Ø IN625 , Ø IN909 , Ø Rene41, Ø HS188
Ø Wasploy, Ø HastelloyX, Ø Nimonic80A, Ø Nimonic263
Ø ...
Main product & Chemical composition:
Nominal composition,%
|
Alloy designation |
Ni |
Cr |
Co |
Mo |
W |
Ta |
Nb |
Al |
Ti |
Fe |
Mn |
Si |
C |
B |
Zr |
|
IN718 |
52.5 |
19 |
|
3 |
|
|
5.1 |
0.5 |
0.9 |
18.5 |
0.2 |
0.2 |
0.04 |
|
|
|
IN625 |
61 |
21.5 |
|
9 |
|
|
3.6 |
0.2 |
0.2 |
2.5 |
0.2 |
0.2 |
0.05 |
|
|
|
Rene41 |
55 |
19 |
11 |
10 |
|
|
|
1.5 |
3.1 |
|
|
|
0.09 |
0.005 |
|
|
Wasploy |
58 |
19.5 |
13.5 |
4.3 |
|
|
|
1.3 |
3 |
|
|
|
0.08 |
0.006 |
0.06 |
|
HastelloyX |
47 |
22 |
1.5 |
9 |
0.6 |
|
|
|
|
18.5 |
0.5 |
0.5 |
0.1 |
|
|
|
Nimonic80A |
76 |
19.5 |
|
|
|
|
|
1.4 |
2.4 |
|
0.3 |
0.3 |
0.06 |
0.003 |
0.6 |
|
Nimonic263 |
51 |
20 |
20 |
5.9 |
|
|
|
0.45 |
2.15 |
|
0.4 |
0.25 |
0.06 |
0.001 |
0.02 |
|
Udimet710 |
55 |
18 |
15 |
3 |
1.5 |
|
|
2.5 |
5 |
|
|
|
0.07 |
0.02 |
|
|
... |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|